In press. Mechanistic switch in corrosion behavior of magnesium alloy diamond lattice structures induced by argon plasma treatment

Viviana M. Posada, Alexandru Marin, Tonny Naranjo, Juan Ramírez, Patricia Fernández-Morales

    Research output: Contribution to journalArticle in an indexed scientific journalpeer-review

    Abstract

    Advancing 3D magnesium (Mg) development beyond current limitations requires controlling Mg alloy degradation in pre-designed, low-dimension architectures. This study reveals a mechanistic switch in the corrosion behavior of Mg alloy (3.6% Al, 0.8 % Zn) diamond lattice structures, induced by plasma nanosynthesis (400 eV Ar+ ions, fluence 1 × 1017 ions/cm2). Plasma treatment of the Mg alloy increases surface Mg from 1.5% to 14.5%, enhances carbonate formation, and generates a nanostructured surface with a Mg carbonate layer over an oxide/hydroxide layer. In vitro and in vivo analyses over 8 wk demonstrate how this treatment fundamentally alters the degradation process and stability of these 3D architectures. While untreated samples initially formed a protective film that subsequently diminished, DPNS-treated samples demonstrated an inverse corrosion behavior. X-ray photoelectron spectroscopy (XPS) and electrochemical impedance spectroscopy (EIS) confirmed the presence of a stable, protective layer composed of magnesium oxide, magnesium hydroxide, and magnesium carbonate on the DPNS-treated surfaces. After 14 days, the DPNS-treated sample exhibited a more positive corrosion potential (-0.69 V versus -1.36 V) and a marginally lower current density (0.73 mA/cm² compared to 0.75 mA/cm²) relative to the control. This protective layer, combined with modified surface topology, initiated a core-to-periphery degradation pattern that maintained structural integrity for up to 8 wk post-implantation. These findings support the conclusion that the DPNS-treated scaffold demonstrates sustained improved corrosion resistance over time compared to the untreated control. Micro-CT revealed plasma-treated samples retained larger struts (504.9 ± 95.3 µm at 8 wk) and formed larger H2 pockets extending 14.2 mm from the implant center, versus 4.9 mm in controls. This corrosion behavior switch enhances stability but risks pore clogging, offering insights for tailoring Mg alloy degradation and H2 evolution in 3D architectures for biomedical applications.

    Original languageEnglish
    JournalJournal of Magnesium and Alloys
    DOIs
    StateAccepted/In press - 2025

    Bibliographical note

    Publisher Copyright:
    © 2025

    Keywords

    • Cellular materials
    • Corrosion resistance
    • Diirected plasma nanosynthesis
    • Mg
    • Nano-medicine
    • Nanotopography

    Fingerprint

    Dive into the research topics of 'In press. Mechanistic switch in corrosion behavior of magnesium alloy diamond lattice structures induced by argon plasma treatment'. Together they form a unique fingerprint.